Waspaloy , Waspaloy da'ay adkaynaya qallafsanaanta superalloy

Faahfaahinta Alaabta

Waspaloy ,
saxan Waspaloy, giraanta Waspaloy, Usha Waspaloy,

Magacyada Ganacsiga Guud: Waspaloy, GH4738, UNS N07001,W.Nr.2.4654.

Waspaloy waa da'da saldhiga nikkel ee la adkeyn karo superalloy leh awood heerkul aad u fiican iyo iska caabin daxalka wanaagsan, gaar ahaan oksaydhka, heerkulka adeega ilaa 1200°F (650°C) ee codsiyada wareega muhiimka ah, iyo ilaa 1600°F (870°C) Codsiyada kale, ka baahi yar.Awoodda heerkulka sare ee daawaha waxaa laga soo qaatay xalkeeda adag ee xoojinaya canaasiirta, molybdenum, cobalt iyo chromium, iyo curiyeyaasha da'da ee adkeynaya, aluminium iyo titanium.Awoodeeda iyo xasiloonideeda ayaa ka sarreeya kuwa sida caadiga ah loo heli karo alloy 718.

 

Halabuurka Kiimikada Waspaloy

C

S

P

Si

Mn

Ti

Ni

Co

Cr

Fe

Zr

Cu

B

Al

Mo

0.02 0.10

≤ 0.015

≤ 0.015

≤ 0.15

≤ 0.10

2.75 3.25

Bal

12.0 15.0

18.0 21.0

≤ 2.0

0.02 0.08

≤ 0.10

0.003 0.01

1.2 1.6

3.5 5.0

Guryaha Jirka ee Waspaloy

Cufnaanta (g/cm3 )

0.296

Barta dhalaalka (℃)

2425-2475

Emperature (℃)

204

537

648

760

871

982

Isku xidhka balaadhinta kulaylka
(gudaha/gudaha °F x 10E-6)

7.0

7.8

8.1

8.4

8.9

9.7

Dhaqdhaqaaqa kulaylka
(Btu • ft/ft2 • saac • °F)

7.3

10.4

11.6

12.7

13.9

-

Hababka Elastic (MPax 10E3)

206

186

179

165

158

144

Waspaloy Alloy Guryaha Makaanikada Caadiga ah

 

Xaalad

Xoog xajin/MPa

Heerkulka shaqada

Xalka baabiinta

800-1000

550ºC

Xalka+gabowga

1300-1500

Annealing

1300-1600

Guga xanaaqsan

1300-1500

¤(Waxqabadka joogtada ah ee heerkulka sare ee caadiga ah, tijaabi xaashida daaweynta kulaylka)

Heerarka Waspaloy iyo Tilmaamaha

 

Baar/Usha /Silig/Fur-saarid Xarig/ Gariir Xaashi/Saxaamo
ASTM B 637, ISO 9723, ISO 9724, SAE AMS 5704, SAE AMS 5706,
SAE AMS 5707, SAE AMS 5708, SAE AMS 5709, SAE AMS 5828,
SAE AMS 5544

Alaabooyinka laga heli karo Waspaloy ee Sekonic Metals

Inconel 718 bar, inconel 625 bar

Baararka Waspaloy & Ulaha

Baararka wareega/ baararka fidsan/ baararka hex, Cabbirka 8.0mm-320mm, Loo isticmaalo boolal, xidhiyaal iyo qaybo kale oo dheeri ah

silig alxanka iyo silig guga

Waspaloy Silig

U keen silig alxanka ah iyo silig guga oo ah qaab gariirad iyo dherer la jaray.

Xaashi & saxan

Waspaloy xaashida & saxan

Balac ilaa 1500mm iyo dhererka ilaa 6000mm, dhumucdiisuna waa 0.1mm ilaa 100mm.

Degdega & Qalab Kale

Xidhayaasha Waspaloy

Walxaha Waspaloy oo ah qaabab Bolts, biro, garabyo iyo kuwa kale oo degdeg ah, marka loo eego qeexitaanka macaamiisha.

inconel strip,invar walaaq,kovar walaaq

Waspaloy strip & gariiradda

Xaalad jilicsan iyo xaalad adag oo leh dusha sare ee AB, ballac ilaa 1000mm

Waa maxay sababta Waspaloy?

 Age adkaynaya daawaha gaarka ah ee nikkel ku salaysan, xoog wax ku ool ah oo sare ee 1400-1600 ° F. Good caabbinta oksaydhka loo isticmaalo engine marawaxadaha gaaska at 1400-1600 ° F jawi.1150-1150 ° F, xoogga dillaaca gurguurta ee Waspaloy ayaa ka sarreeya 718.

Miisaanka 0-1350 ° F, xoogga jilicsanaanta kulul ee wakhti gaaban ayaa ka xun 718 aloy

Goobta Codsiga ee Waspaloy:

Waspaloy waxaa loo isticmaalaa qaybaha matoorada marawaxadaha gaaska kuwaas oo u yeera xoog badan iyo iska caabin daxalka ee heerkulka shaqada sare. Hadda iyo codsiyada suurtagalka ah waxaa ka mid ah kombaresarada iyo saxannada rotor, shafts, spacers, shaabadihii, giraangiraha iyo daasadaha, xirmooyinka iyo qalab kale oo kala duwan ee mishiinka, shirarka hawada. iyo hababka gantaalada.

 

Waspaloy waa da'da-engegan superalloy qallafsan, heerkulka hawlgalka ma dhaafo 815 ℃. Alloy wuxuu leeyahay xoog dhalidda sare iyo iska caabin daal at 760 ℃ ~ 870 ℃, iyo oksidation sare iyo iska caabin daxalka at 870 ℃, kaas oo ku haboon wax soo saarka WO discs. Mashiinnada shaqada, xirmooyinka heerkulka sare, dhululubada ololka, shafts iyo kiisaska marawaxadaha WO. Alaabooyinka ugu muhiimsan waa xariijimo qabow iyo xaashi duuban oo kulul, tuubo, xariijimo, fiilada, foornada iyo xirmooyinka boodhka, iwm.
Summada u dhiganta: W.nr 2.4654, UNS N07001, AWS 170
Heerka lagu dabaqi karo: AMS 5544 AMS 5708 AMS 5828


  • Hore:
  • Xiga:

  • Halkan ku qor fariintaada oo noo soo dir